Advanced Search+
ZHUANG Ren-ai, ZHANG Wei-gang, LI Yan-jun, WANG Shu-qiang, WANG Li, PANG Xiao-ren. Effect of Hot Water Treatment on Color Fastness and Surface of Reconstituted Bamboo Lumber[J]. Journal of Zhejiang Forestry Science and Technology, 2016, 36(2): 54-57.
Citation: ZHUANG Ren-ai, ZHANG Wei-gang, LI Yan-jun, WANG Shu-qiang, WANG Li, PANG Xiao-ren. Effect of Hot Water Treatment on Color Fastness and Surface of Reconstituted Bamboo Lumber[J]. Journal of Zhejiang Forestry Science and Technology, 2016, 36(2): 54-57.

Effect of Hot Water Treatment on Color Fastness and Surface of Reconstituted Bamboo Lumber

More Information
  • Received Date: August 08, 2015
  • Revised Date: January 17, 2016
  • Bamboo bundles were hot water treated at 120, 140, 160℃ with duration of 60 minutes, and at 160℃ with duration of 30, 60 and 90 minutes, and then treated bundles were pressed to reconstituted bamboo lumber(RBL). Color fastness of RBL was tested by climate chamber, and surface of RBL was observed by SEM. The results showed that the color fastness of RBL increased with temperature, the minimum color difference under 160℃ was 9.1, and treatment duration had no evident effect on color fastness. SEM demonstrated that surface of treated RBL was damaged compared with no treatment.
  • [1]
    赵仁杰,喻云水. 竹材人造板工艺学[M]. 北京:中国林业出版社,2002.
    [2]
    张自斌,周光益,林亲众. 我国丛生竹研究进展与问题探讨[J]. 热带林业,2007,35(2):12-15.
    [3]
    赵鹤,张建,李琴. 竹材防霉防腐研究现状及发展趋势[J]. 山西建筑,2010,36(29):137-139.
    [4]
    孙芳利,段新芳. 竹材防霉研究状况及其展望[J]. 世界竹藤通讯,2004,2(4):1-4.
    [5]
    秦莉,于文吉. 重组竹材研究现状与展望[J]. 世界林业研究,2009,22(6):55-59.
    [6]
    Wiland J J,Guyonnet R. Study of chemical modifications and fungi degradation of thermally modified wood using DRIFT spectroscopy[J]. Holz Roh Werstoff, 2003,61(3):216-220.
    [7]
    Kamdem D P,Pizzi A, Jermannaud A. Durability of heat-treated wood[J]. Holz Roh Werstoff, 2002,60(1):1-6
    [8]
    Mets-Kortelainen S, Antikainen T, Viitaniemi P. The water absorption of sapwood and heartwood of Scots pine and Norway spruce heat-treated at 170℃,190℃,210℃ and 230℃[J]. Holz Roh Werkstoff, 2006,64(3):192-197.

Catalog

    Article views (435) PDF downloads (269) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return